Mechanical Properties Metric English Comments
Flexural Yield Strength 176 - 227 MPa
25500 - 32900 psi
Average value: 203 MPa Grade Count:16
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E..
Flexural Yield Strength 80.0 - 227 MPa

@Temperature 100 - 175 °C
11600 - 32900 psi

@Temperature 212 - 347 °F
Average value: 129 MPa Grade Count:8
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..