Flexural Yield Strength 244 MPa
35400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP WX93111 PBT (Europe-Africa-Middle East)
LNP* THERMOCOMP* WX93111 is a compound based on Polybutylene Terephalate resin containing Flame retardant , Glass Fiber, Proprietary filler. Added features include : Improved CTI.
Flexural Yield Strength 244 MPa

@Temperature 175 °C
35400 psi

@Temperature 347 °F
After ageing at 70°C / 95% RH
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix
5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel