Mechanical Properties Metric English Comments
Flexural Yield Strength 107 - 372 MPa
15500 - 54000 psi
Average value: 260 MPa Grade Count:82
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Flexural Yield Strength 89.6 - 372 MPa
13000 - 54000 psi
Average value: 249 MPa Grade Count:13
Overview of materials for Nylon 610, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of..