Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 179 - 432 MPa | 26000 - 62700 psi | Average value: 295 MPa Grade Count:18 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Yield Strength | 26.0 - 432 MPa | 3770 - 62700 psi | Average value: 190 MPa Grade Count:6 |
Overview of materials for Thermoset Polyurethane Foam, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Glass Filled". Each property range of values reported is minimum and maximu.. |