Mechanical Properties Metric English Comments
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Solvay Specialty Polymers Veradel® AG-230 Polyethersulfone  (discontinued **)
For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N..
Flexural Yield Strength 179 - 432 MPa
26000 - 62700 psi
Average value: 295 MPa Grade Count:18
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Techmer ES Electrablend® PC CF20 CR X 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Good Chemical Resistance and Semi ConductiveInformation provided by TP Compos..
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Techmer ES Electrablend® PC CF20 FR IM BK 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Frame Retardant, Impact Modified and Semi Conductive..
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Techmer ES Electrablend® PC/PET CF20 IM 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact Modified and Semi ConductiveAppearance: Black..
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Techmer ES HiFill® PP LGF50 CC NAT 12mm 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass Fiber, 50% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Techmer ES HiFill® PPS/F GF/M35 X 35% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Yield Strength 179 MPa
26000 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF006RXQ PC
LNP* THERMOCOMP* DF006RXQ is a compound based on Polycarbonate resin containing 30% Glass Fiber.
Flexural Yield Strength 179 MPa
26000 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP KF008 Acetal Copolymer (Europe-Africa-Middle East)
LNP* THERMOCOMP* KF008 is a compound based on Acetal Copolymer resin containing Glass Fiber.
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Techmer ES HiFill® PP GF50 CC HF BK 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc...
Flexural Yield Strength 179 MPa
26000 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp LFZ42XXC PEEK
LNP THERMOCOMP* LFZ42XXC is a compound based on Polyetheretherketone resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage.This data was supplied by SABIC..
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
PlastxWorld CEVIAN® A2606 30% GF PA/ABS Alloy, DAM
Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Clariant Renol 612G20-L Nylon 612, 20% Glass Fiber Reinforced, Lubricated
Data provided by Clariant Masterbatches
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Clariant Renol PA133G33 Nylon 66, 33% Glass Fiber, Highly Impact Modified
Data provided by Clariant Masterbatches
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Ascend Performance Materials VYDYNE® R513 Nylon, 13% Glass Reinforced
Typical property data. VYDYNE is a registered trademark of Solutia Inc.
Flexural Yield Strength 179 - 221 MPa
26000 - 32000 psi
Average value: 200 MPa Grade Count:10
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma..
Flexural Yield Strength 179 MPa
26000 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC
LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated.
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Techmer ES HiFill® PP LGF40 CC HS BK 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Chemically Coupled and Heat StabilizedAppearance: Bla..