Mechanical Properties Metric English Comments
Flexural Yield Strength 300 MPa
43500 psi
ISO 178, ASTM D790
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte..
Flexural Yield Strength 300 MPa
43500 psi
ASTM D790
E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET
45% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd.
Flexural Yield Strength 300 MPa
43500 psi
ASTM Data
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he..