Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 317 MPa | 46000 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Flexural Yield Strength | 317 MPa | 46000 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Flexural Yield Strength | 317 MPa | 46000 psi | ASTM D790 |
Techmer ES Electrafil® J-3/CF/30 Nylon 6, 30% Carbon Fiber Reinforced |
|||
Flexural Yield Strength | 317 MPa | 46000 psi | ASTM D790 |
Clariant Renol PA213G50 Nylon 6, 50% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |