Polymer Property : Flexural Yield Strength = 50.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 50.0 - 50.0 MPa

@Temperature 90.0 - 90.0 °C
7250 - 7250 psi

@Temperature 194 - 194 °F
Average value: 50.0 MPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..