Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 3.45 - 68.9 MPa | 500 - 10000 psi | Average value: 22.2 MPa Grade Count:32 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Yield Strength | 3.45 - 56.0 MPa | 500 - 8130 psi | Average value: 31.0 MPa Grade Count:16 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |