Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 44.2 MPa | 6410 psi | 15 mm/min; ASTM D790 |
LG Chemical SI-610 Alphalac Polystyrene High flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include big size electric app.. |
|||
Flexural Yield Strength | 44.2 MPa | 6410 psi | 15 mm/min; ASTM D790 |
LG Chemical 401 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, uses non-bromide as fl.. |