Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 73.5 MPa @Thickness 3.20 mm |
10700 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical HIPS MI730 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Flexural Yield Strength | 73.5 MPa @Thickness 3.20 mm |
10700 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical LG703W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided.. |
|||
Flexural Yield Strength | 73.5 MPa @Thickness 3.20 mm |
10700 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical LG749W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by.. |
|||
Flexural Yield Strength | 73.5 MPa @Thickness 3.20 mm |
10700 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LI942 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical |
|||
Flexural Yield Strength | 73.5 MPa @Thickness 3.20 mm |
10700 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® HV1005S PBT Description: Injection Molding, PBT, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 73.5 MPa | 10700 psi | ASTM D790 |
GRECO ISOPAK 547 ABS Resin High Impact GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Flexural Yield Strength | 73.5 MPa @Thickness 6.40 mm |
10700 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical TR556 MABS, Transparency, Chemical Resistance Feature: Injection Molding, Transparency, Chemical ResistanceApplication: Sound Proofing Wall, Canopy, Other Transparent SheetsCAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical.. |
|||
Flexural Yield Strength | 73.5 MPa @Thickness 3.20 mm |
10700 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Flexural Yield Strength | 73.5 MPa @Thickness 3.20 mm |
10700 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR474 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior HousingCAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Flexural Yield Strength | 73.5 MPa | 10700 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN173HI3R High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Yield Strength | 73.5 MPa | 10700 psi | ASTM D790 |
Samyang Tribit® 1503S Polybutylene Terephthalate Characteristics:High impactApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samyang |
|||
Flexural Yield Strength | 73.5 MPa | 10700 psi | ASTM D790 |
Samyang Tribit® 1510 PBT, Middle Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1510 is a middle viscosity grade.Informatio.. |
|||
Flexural Yield Strength | 73.5 MPa | 10700 psi | ASTM D790 |
Samyang Triloy® 170 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityFlame retardantApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Flexural Yield Strength | 73.5 MPa @Thickness 6.40 mm |
10700 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM21V ABS Injection Molding Grade Super High Gloss, High RigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 73.5 MPa @Thickness 6.40 mm |
10700 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM21V ABS Injection Molding Grade Super High Gloss, High RigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 73.5 MPa @Thickness 3.20 mm |
10700 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 73.5 MPa @Thickness 3.20 mm |
10700 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical SG175G ABS, Super Surface Gloss, High Flow Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |