Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical TR556 MABS, Transparency, Chemical Resistance

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical TR556 MABS, Transparency, Chemical Resistance.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Feature: Injection Molding, Transparency, Chemical ResistanceApplication: Sound Proofing Wall, Canopy, Other Transparent SheetsCAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Melt Flow 4.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
4.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength, Yield 47.1 MPa

@Thickness 3.20 mm
6830 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break 30 %

@Thickness 3.20 mm
30 %

@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Yield Strength 73.5 MPa

@Thickness 6.40 mm
10700 psi

@Thickness 0.252 in
15 mm/min; ASTM D790
Flexural Modulus 2.16 GPa

@Thickness 6.40 mm
313 ksi

@Thickness 0.252 in
15 mm/min; ASTM D790
Izod Impact, Notched 1.77 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
3.31 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
1.77 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
3.31 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C

@Thickness 6.40 mm
185 °F

@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical 50.0 °C

@Thickness >=1.50 mm
122 °F

@Thickness >=0.0591 in
50.0 °C

@Thickness >=3.00 mm
122 °F

@Thickness >=0.118 in
UL RTI, Mechanical with Impact 50.0 °C

@Thickness >=1.50 mm
122 °F

@Thickness >=0.0591 in
50.0 °C

@Thickness >=3.00 mm
122 °F

@Thickness >=0.118 in
UL RTI, Mechanical without Impact 50.0 °C

@Thickness >=1.50 mm
122 °F

@Thickness >=0.0591 in
50.0 °C

@Thickness >=3.00 mm
122 °F

@Thickness >=0.118 in
Flammability, UL94 HB

@Thickness >=1.50 mm
HB

@Thickness >=0.0591 in
HB

@Thickness >=3.00 mm
HB

@Thickness >=0.118 in
Optical Properties Metric English Comments
Haze 2.6 %
2.6 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003
Users viewing this material also viewed the following: