Polymer Property : Flexural Yield Strength = 8400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 57.9 MPa
8400 psi
ASTM D790
Ineos ABS Lustran® QE 1094 AS General Purpose, High-Impact  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La..
Flexural Yield Strength 57.9 - 343 MPa
8400 - 49700 psi
Average value: 229 MPa Grade Count:18
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..
Flexural Yield Strength 57.9 MPa
8400 psi
ASTM D790
PlastxWorld CEVIAN® E10 Inherently Static Dissipative ABS
Inherently Static Dissipative ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Yield Strength 57.9 MPa
8400 psi
ASTM D790
PlastxWorld Veroplas PA2002HI Nylon 6
general purpose, unfilled, high impact modified injection molding gradeInformation provided by PlastxWorld Inc.