Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 88.1 MPa | 12800 psi | ASTM D790 |
Plenco Valite 4100 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac.. |