Polymer Property : Flexural Yield Strength = 8800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 60.7 MPa
8800 psi
ASTM D790
Ravago Manufacturing Americas Hylac® FR134 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Flexural Yield Strength 60.7 MPa
8800 psi
ASTM D790
Ravago Manufacturing Americas Hylac® GP48 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Flexural Yield Strength 60.7 MPa
8800 psi
ASTM D790
Techmer ES HiFill® TPX-PVDF-03009 C
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerFeatures: Low Shrinkage and Low Smoke EmissionInformation provided by TP Composites, Inc.
Flexural Yield Strength 60.7 MPa
8800 psi
ASTM D790
PlastxWorld CEVIAN® A1500 PA/ABS Alloy, DAM
Property data is for dry as molded (DAM) samples.Information provided by PlastxWorld Inc.