Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 64.8 MPa | 9400 psi | ASTM D790 |
Ineos ABS Lustran® 1148 General Purpose, High-Impact
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
Flexural Yield Strength | 64.8 MPa | 9400 psi | ASTM D790 |
Spartech Royalite R47 PVC Alloy Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 64.8 MPa | 9400 psi | ASTM D790 |
Spartech Royalite R570 FR-ABS Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 64.8 MPa | 9400 psi | ASTM D790 |
Techmer ES Plastiblend® ABS 92RK Availability: North AmericaForms: PelletsFeatures: General PurposeProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 64.8 MPa | 9400 psi | ASTM D790 |
Techmer ES Plastiblend® ABS CR X Availability: North AmericaForms: PelletsFeatures: Good Chemical ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 64.8 MPa | 9400 psi | |
Abatron AboCast 50-16/AboCure 50-1 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/35 ratio. Pot life: 500 g, 380 min. at 25°C (77°F). Exothermic Peak 154°C (310°F). Hardens in 2-24 hour.. |
|||
Flexural Yield Strength | 64.8 MPa | 9400 psi | ASTM D790 |
PlastxWorld Veroplas PA2002MI Nylon 6 general purpose, unfilled, medium impact modified injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 64.8 MPa | 9400 psi | ASTM D790 |
Spartech Soft Touch PPR Co-Extruded Polyolefin Skin/PPR Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |