Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 97.5 MPa | 14100 psi | Plain Cast Resin; ASTM D790 |
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Flexural Yield Strength | 97.5 MPa | 14100 psi | Plain Cast Resin; ASTM D790 |
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |