Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 67.7 MPa | 9810 psi | ASTM D790 |
GRECO ISOPAK 547M ABS Resin Metal Plating GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Flexural Yield Strength | 67.7 MPa @Thickness 6.40 mm |
9810 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Flexural Yield Strength | 67.7 MPa @Thickness 6.40 mm |
9810 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU650N ABS Heat Resistant Medium/High ImpactInformation provided by Bhansali |
|||
Flexural Yield Strength | 67.7 MPa | 9810 psi | ASTM D790 |
Cheng Yu Plastic 3285 TPE Rubber |
|||
Flexural Yield Strength | 67.7 MPa @Thickness 6.40 mm |
9810 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU650N ABS Heat Resistant Medium/High ImpactInformation provided by Bhansali |
|||
Flexural Yield Strength | 67.7 MPa @Thickness 6.40 mm |
9810 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |