Polymer Property : 1% Secant Modulus, MD = 1030 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 1030 MPa
150000 psi
ASTM D882
ExxonMobil HDPE HD 7925.30 High Density Polyethylene Resin
Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.A..
1% Secant Modulus, MD 1030 MPa
150000 psi
ASTM D882
ExxonMobil HDPE HD 7960..13 High Density Polyethylene Resin
Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 ..
1% Secant Modulus, MD 1030 MPa
150000 psi
ASTM D882
ExxonMobil HD 7925.30 Barrier Film Resin
Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.A..
1% Secant Modulus, MD 1030 MPa
150000 psi
ASTM D882
ExxonMobil HD 7960.13 HMW Blown Film Resin
Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 ..
1% Secant Modulus, MD 1030 MPa
150000 psi
ASTM D882
ExxonMobil Paxon™ 4700 Blown Film Extrusion Resin  (discontinued **)
4700 is a medium molecular weight, high density polyethylene homopolymer film resin. It can be processed on conventional film extrusion equipment.Information provided by ExxonMobil Chemical