Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 1% Secant Modulus, MD = 145 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 145 MPa
21000 psi
ISO 527-3
Polimeri Europa Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T CMH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CMH 108 show e..
1% Secant Modulus, MD 145 MPa
21000 psi
ASTM D882
ExxonMobil LD 135.09 Cast Packaging Film Resin  (discontinued **)
LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging..
1% Secant Modulus, MD 145 MPa
21000 psi
ASTM D882
Westlake EF444 4.7% Ethylene Vinyl Acetate Copolymer  (discontinued **)
Excellent haze and gloss, excellent impact strength and very good sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, section 177..
1% Secant Modulus, MD 145 MPa
21000 psi
ASTM D882
LyondellBasell Petrothene® NA340141 Low Density Polyethylene
ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea..
1% Secant Modulus, MD 145 MPa
21000 psi
ASTM D882
LyondellBasell Petrothene® NA340163 Low Density Polyethylene
ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea..
1% Secant Modulus, MD 145 MPa
21000 psi
ASTM E111
LyondellBasell Petrothene® NA340185 Low Density Polyethylene, Film Extrusion Grade
PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea..
1% Secant Modulus, MD 145 MPa
21000 psi
ASTM E111
LyondellBasell Petrothene® NA340212 Low Density Polyethylene, Film Extrusion Grade
PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea..
1% Secant Modulus, MD 145 MPa
21000 psi
ASTM D882
LyondellBasell Petrothene® NA340013 Low Density Polyethylene
ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea..
1% Secant Modulus, MD 145 MPa
21000 psi
ASTM D882
Westlake Elevate™ EF439 4.0% Ethylene Vinyl Acetate Copolymer
Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio..
1% Secant Modulus, MD 145 MPa
21000 psi
ASTM D882
ExxonMobil Exceed™ 1015HA Metallocene Polyethylene Resin
Product Description: Exceed 1015 mVLDPE resin is metallocene ethylene-hexene copolymer. Films made from Exceed 1015 mVLDPE have outstanding cold temperature toughness, impact strength and puncture. ..
1% Secant Modulus, MD 145 MPa
21000 psi
ASTM D882
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin
Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren..
1% Secant Modulus, MD 145 MPa
21000 psi
ASTM D882
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin (European Grade)
Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high clarity film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impa..
1% Secant Modulus, MD 145 MPa
21000 psi
ASTM D882
ExxonMobil LDPE LD 302.56 Low Density Polyethylene Resin
Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren..
Copyright © lookpolymers.com All Rights Reserved