Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 110 MPa | 15900 psi | ASTM D882 |
ExxonMobil LL 3002.32 Cast Film Resin
(discontinued **) LL 3002.32 is a hexene copolymer LLDPE cast film resin. Films produced from this resin have excellent tensile properties, as well as stiffness and toughness. Combined with good drawdown properties, .. |
|||
1% Secant Modulus, MD | 110 MPa | 15900 psi | ASTM D882 |
ExxonMobil Escorene® LD 713.93 Cast Film Resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhbits very high impact strength, hihg clarity, and excellent heat sealabilityAvailability: Latin.. |