Polymer Property : 1% Secant Modulus, MD = 262 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 262 MPa
38000 psi
ASTM D882
LyondellBasell Petrothene® NA285003 Medium Density Polyethylene
ApplicationsPETROTHENE NA 285-003 is a medium density polyethylene resin for blown or cast film extrusion. Typical applications include overwrap film. This product exhibits good film optics and hi..
1% Secant Modulus, MD 262 MPa
38000 psi
ASTM D882
LyondellBasell Petrothene® NA324009 Low Density Polyethylene (Film Grade)
ApplicationsPETROTHENE NA 324 is a series of homopolymer resins specifically designed for overwrap packaging. NA 324 provides excellent optical properties and good stiffness for improved machineabi..
1% Secant Modulus, MD 262 MPa
38000 psi
ASTM D882
ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin
Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.A..