Polymer Property : 1% Secant Modulus, MD = 51.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 51.0 MPa
7400 psi
ASTM D882
ExxonMobil Escorene™ FL 00018 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00018 is a copolymer of ethylene and vinyl acetate. It offers combines toughness, good optical and sealing properties and low gel. In particular, its good behavior in high fr..
1% Secant Modulus, MD 51.0 MPa
7400 psi
ASTM D882
ExxonMobil Escorene™ LD 723.28 Cast Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra UL 723.28 is a high VA extrusion coating resin, which provides outstanding heat sealability and high clarity. LD 723.28 has a good balance of drawabilty and neck-..
1% Secant Modulus, MD 51.0 MPa
7400 psi
ASTM D882
ExxonMobil Escorene™ UL 00018 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00018 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic..
1% Secant Modulus, MD 51.0 MPa
7400 psi
ASTM D882
ExxonMobil Optema® TC-110 Cast Ethylene Methyl Acrylate
Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It can produce f..