Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 40.0 MPa | 5800 psi | ISO 527-3 |
Polimeri Europa Clearflex® CL D0 Very Low Density Polyethylene Clearflex CL D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).This resin is produced with a proprietary technology. Stretch films manufactured.. |