Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 450 MPa | 65300 psi | ISO 527-3 |
Polimeri Europa Clearflex® FH 50 Linear Medium Density Polyethylene Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FH 50 are characterized by a good balance between toug.. |
|||
1% Secant Modulus, MD | 450 MPa | 65300 psi | ASTM-D882 |
Braskem LL3800N HDPE Cast Film Extrusion Polyethylene Copolymer The resin LL3800N is a high-density polyethylene, copolymer octene-1, produced by the solution process for the extrusion of plain films with excellent mechanical properties. It has an antirust addit.. |