Polymer Property : 1% Secant Modulus, MD = 96.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 96.5 MPa
14000 psi
ASTM D882
Westlake DA591 9.0% Ethylene Vinyl Acetate Copolymer
Westlake DA591 resin is a 9.0% EVA copolymer designed as a tie layer in multi-layered food packaging film. It has excellent clarity, excellent toughness, good resistance to load deformation, and goo..
1% Secant Modulus, MD 96.5 MPa
14000 psi
D 882
Westlake EB591 9.0% Ethylene Vinyl Acetate Copolymer
Westlake EB591 resin is a 9.0% EVA copolymer designed for ice bags, frozen food bags and other films that require excellent toughness and good heat sealing characteristics. This kosher compliant re..
1% Secant Modulus, MD 96.5 MPa
14000 psi
ASTM-D882
Westlake Elevate™ EB591 9% EVA Copolymer
Westlake EB591 resin is a 9% EVA copolymer designed for films that require excellent toughness and good heat sealing characteristics. This Kosher compliant resin has excellent low temperature brittl..
1% Secant Modulus, MD 96.5 MPa
14000 psi
ASTM D882
Westlake Elevate™ EF563 6.5% Ethylene Vinyl Acetate Copolymer
Westlake EF 563 resin is a fractional melt index 6.5% EVA copolymer with excellent drawdown, low melting/dispersion, and clarity optics in a soft but very tough film. Kosher compliant.Application/U..