Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 965 MPa | 140000 psi | ASTM D882 |
ExxonMobil HDPE HTA 002 High Density Polyethylene Resin Product Description: HTA 002 is a general purpose medium molecular weight HDPE grade, characterized by easy processability, especially in coextrusion and blending with other polyolefins. HTA 002 can.. |