Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 101 MPa | 14600 psi | ASTM D882 |
ExxonMobil Escorene® LD 713.93 Cast Film Resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhbits very high impact strength, hihg clarity, and excellent heat sealabilityAvailability: Latin.. |