Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 758 MPa | 110000 psi | ASTM E111 |
LyondellBasell Petrothene® LP540200 High Density Polyethylene, Film Extrusion Grade PETROTHENE LP540200 is a copolymer resin designed for blown film applications. This resin offers high ESCR, stiffness, excellent appearance and bubble stability. LP540200 is recommended for high str.. |
|||
1% Secant Modulus, TD | 758 MPa | 110000 psi | ASTM D882 |
LyondellBasell Petrothene® LP540200 High Density Polyethylene ApplicationsPETROTHENE LP 5402-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good draw-down. LP 5402-0.. |