Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 800 MPa | 116000 psi | ISO 527-3 |
Polimeri Europa Eraclene® FC 82 High Density Polyethylene - Blown Film Extrusion Eraclene FC 82 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully co.. |