Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 131 MPa | 19000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012 MJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
1% Secant Modulus, TD | 131 MPa | 19000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
1% Secant Modulus, TD | 131 MPa | 19000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001.32 Linear Low Density Polyethylene Resin Product Description: LL 1001.32 is a butane LLDPE resin. Films made from LL 1001.32 have very good tensile and toughness properties.Availability: Latin America, North America and South America Addit.. |
|||
1% Secant Modulus, TD | 131 MPa | 19000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002YB Cast Linear Low Density Polyethylene Resin Product Description: LL 1002YB is an LLDPE resin designed for cast films. It offers high gloss and excellent drawdown in both blown and cast film applications. LL 1002YB may also be used as a blend .. |
|||
1% Secant Modulus, TD | 131 MPa | 19000 psi | ASTM D882 |
ExxonMobil Exceed™ 3518CB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 3518CB is a metallocene ethylene-hexene copolymer. Films made of Exceed 3518CB grade have outstanding tensile, impact and puncture resistance properties. Furthermore, the.. |