Polymer Property : 1% Secant Modulus, TD = 140000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 965 MPa
140000 psi
ASTM D822
LyondellBasell Alathon® L5845 High Density Polyethylene
ApplicationsALATHON L 5845 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include paper replacement, coextrusions and laminations.Reg..
1% Secant Modulus, TD 965 MPa
140000 psi
ASTM D822
LyondellBasell Alathon® L5005 High Density Polyethylene
ApplicationsALATHON L 5005 is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typi..