Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 965 MPa | 140000 psi | ASTM D822 |
LyondellBasell Alathon® L5845 High Density Polyethylene ApplicationsALATHON L 5845 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include paper replacement, coextrusions and laminations.Reg.. |
|||
1% Secant Modulus, TD | 965 MPa | 140000 psi | ASTM D822 |
LyondellBasell Alathon® L5005 High Density Polyethylene ApplicationsALATHON L 5005 is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typi.. |