Polymer Property : 1% Secant Modulus, TD = 1600 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 1600 MPa
232000 psi
ASTM D882
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer
Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films..