Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 1600 MPa | 232000 psi | ASTM D882 |
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films.. |