Polymer Property : 1% Secant Modulus, TD = 197 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 197 MPa
28600 psi
ASTM D882
ExxonMobil LD 071.MU Blown Film Resin  (discontinued **)
LD 071 series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, toughness, burn-through re..
1% Secant Modulus, TD 197 MPa
28600 psi
Cast; ASTM D882
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
1% Secant Modulus, TD 197 MPa
28600 psi
Cast; ASTM D882
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..