Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 212 MPa | 30800 psi | ASTM D882 |
ExxonMobil LD 146.NH Cast Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
1% Secant Modulus, TD | 212 MPa | 30800 psi | ASTM D882 |
ExxonMobil LD 146.NH Packaging Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |