Polymer Property : 1% Secant Modulus, TD = 30800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 212 MPa
30800 psi
ASTM D882
ExxonMobil LD 146.NH Cast Film Resin  (discontinued **)
LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical
1% Secant Modulus, TD 212 MPa
30800 psi
ASTM D882
ExxonMobil LD 146.NH Packaging Film Resin  (discontinued **)
LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical