Polymer Property : 1% Secant Modulus, TD = 240 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 240 MPa
34800 psi
ASTM D882
SABIC 218B Linear Low Density Polyethylene for Cast Film
Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u..
1% Secant Modulus, TD 240 MPa
34800 psi
ISO 527-3
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability..
1% Secant Modulus, TD 240 MPa
34800 psi
ASTM D882
Braskem Green PE SLH218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability..
1% Secant Modulus, TD 240 MPa
34800 psi
ASTM D882
Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene
Description: LH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability...