Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LL 1235x70 Cast Film Resin
(discontinued **) LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
LyondellBasell Petrothene® NA420127 Low Density Polyethylene
(discontinued **) ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | Blown; ASTM D882 |
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
LyondellBasell Petrothene® NA420000 Low Density Polyethylene ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | Blown; ASTM D882 |
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM E111 |
LyondellBasell Petrothene® NA426225 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA426 is a series of LDPE/EVA copolymer resins for high impact and clarity packaging film. These resins exhibit excellent a broad range of extrusion conditions. Well-balanced films with e.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
Westlake Mxsten CV77518 Polyethylene Plastomer Mxsten CV Plastomer CV77518 resin is a polyethylene plastomer designed for blown and cast film extrusion that contains no slip and no antiblock additives. Films produced with this resin exhibit a ve.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882, A |
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Film Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityExcellent tear strengthHigh puncture resistanceGood stiffnessExcellent heat sealing proper.. |
|||
1% Secant Modulus, TD | 172 MPa @Thickness 0.0254 mm |
25000 psi @Thickness 0.00100 in |
ASTM D882A |
Total Lumicene® mPE M 3410 EP HDPE Film Outstanding clarity and gloss; excellent bubble stability; excellent tear strength; high puncture resistance; good stiffness; excellent heat sealing properties; excellent compatibility with LDPE and.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil Exceed™ 2018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018EB is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films. Availability: Africa & Middl.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LD331.08 EVA LD 331.08 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LD331.99 EVA LD 331.99 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LDPE LD 364HE Low Density Polyethylene Resin Product Description: LD 364HE is an LDPE, offering a good combination of mechanical, optical and sealing properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1500 ppmSlip: .. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin (European Grade) Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high clarity film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impa.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LDPE LD 302.56 Low Density Polyethylene Resin Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren.. |