Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA420000 Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA420000 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Well-balance films with excellent optics, good stiffness and strong heat sealing characters can be produced from this resin. Regulatory StatusNA 420 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1350. This regulation allows the use of this ethylene vinyl acetate copolymer "…in articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesNA 420 has excellent drawdown characteristics that yield outstanding output rates. Recommended extrusion conditions are 330°-380°F (166°-194°C) melt temperatures and a blow-up ratio between 1.7-3.0:1. Specific recommendations for the processing of NA 420 can be made only when the end use application, required properties and the processing equipment are known. For exact recommendations, please contact your Equistar representative.Physical PropertiesThese are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 8"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron) gauge, 0.025"die gap at 130 lb/hr.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D1505
Vinyl Acetate Content 2.5 %
2.5 %
Thickness 31.8 microns
1.25 mil
2:1 BUR; 25 mil die gap
Melt Flow 2.5 g/10 min
2.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 350 %
350 %
ASTM D882
Film Elongation at Break, TD 550 %
550 %
ASTM D882
Elmendorf Tear Strength MD 220 g
220 g
ASTM D1922
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
Dart Drop Test 80.0 g
0.176 lb
F<sub>50</sub>; ASTM D1709
Film Tensile Strength at Break, MD 22.8 MPa
3300 psi
ASTM D882
Film Tensile Strength at Break, TD 16.5 MPa
2400 psi
ASTM D882
1% Secant Modulus, MD 138 MPa
20000 psi
ASTM D882
1% Secant Modulus, TD 172 MPa
25000 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 4.5 %
4.5 %
Optical properties are given for NA 420-127 (medium-slip, medium antiblock).; ASTM D1003
Gloss 73 %
73 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F
Descriptive Properties Value Comments
Antiblock None
Slip None