Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 1% Secant Modulus, TD = 290 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 290 MPa
42100 psi
ISO 527-3
Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an..
1% Secant Modulus, TD 290 MPa
42100 psi
ISO 527-3
Polimeri Europa Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 30 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 U are characterized b..
1% Secant Modulus, TD 290 MPa
42000 psi
ASTM D882
Westlake LF2010 Hexene Linear Low Density Polyethylene
Westlake LF2010 is a hexene LLDPE with increased stiffness suitable for heavy duty films and shipping sacks. This material contains process aid for improved ease of extrusion, and can be blended wit..
1% Secant Modulus, TD 290 MPa
42000 psi
ASTM D882
ExxonMobil LD 071.LQ Blown Film Resin
L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou..
1% Secant Modulus, TD 290 MPa
42000 psi
ASTM D882
ExxonMobil LD 071.LR Blown Film Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
1% Secant Modulus, TD 290 MPa
42000 psi
ASTM D882
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
1% Secant Modulus, TD 290 MPa
42000 psi
ASTM D882
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
1% Secant Modulus, TD 290 MPa
42000 psi
ASTM D882
ExxonMobil LDPE LD 156BW Low Density Polyethylene Resin
Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo..
1% Secant Modulus, TD 290 MPa
42000 psi
ASTM D882
ExxonMobil LDPE LD 156HE Low Density Polyethylene Resin
Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo..
Copyright © lookpolymers.com All Rights Reserved