Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 50.0 MPa | 7250 psi | ISO 527-3 |
Polimeri Europa Clearflex® CL D0 Very Low Density Polyethylene Clearflex CL D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).This resin is produced with a proprietary technology. Stretch films manufactured.. |