Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 50.3 MPa | 7300 psi | D882 |
Westlake EF528 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF528 is an ethylene vinyl acetate copolymer with 18.5% VA. EF528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength .. |
|||
1% Secant Modulus, TD | 50.3 MPa | 7300 psi | ASTM D882 |
Westlake Elevate™ DA528AA 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength.. |
|||
1% Secant Modulus, TD | 50.3 MPa | 7300 psi | ASTM D882 |
Westlake Elevate™ DA528AA Ethylene Vinyl Acetate Copolymer Developmental ProductDescription: Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat s.. |
|||
1% Secant Modulus, TD | 50.3 MPa | 7300 psi | D882 |
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF529 is an ethylene vinyl acetate copolymer with 18.5% VA. It contains no slip or antiblock and is designed for blown and cast films requiring excellent optics and low heat seal .. |
|||
1% Secant Modulus, TD | 50.3 MPa | 7300 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00218 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00218 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation. Machines should always b.. |