Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 386 MPa | 56000 psi | ASTM D882 |
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, TD | 386 MPa | 56000 psi | ASTM D882 |
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
1% Secant Modulus, TD | 386 MPa | 56000 psi | ASTM D882 |
ExxonMobil LD 129.24 Cast Overwrap Film Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
1% Secant Modulus, TD | 386 MPa | 56000 psi | ASTM D882 |
ExxonMobil LDPE LD 129.24 Low Density Polyethylene Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
1% Secant Modulus, TD | 386 MPa | 56000 psi | ASTM D882, A |
Total Lumicene® mPE M 3410 EP Metallocene Medium Density Film Resin
(Unverified Data**) Polyethylene: Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityHigh StiffnessGood puncture resistanceGood tear strengthGood heat sealing p.. |