Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 60.7 MPa | 8800 psi | ASTM D882 |
ExxonMobil Exact™ 4151 Ethylene-based Plastomer Resin Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer and multilayer coe.. |