Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 1500 g/25 mm | 1500 g/in | PP, bar temp 150-175°C |
DuPont Appeel® LSR 1184 Modified EVA Lidding Sealing Resin
(discontinued **) Appeel® 1184 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc.. |
|||
Seal Strength | 1500 g/25 mm | 1500 g/in | seal bar 125°C. |
DuPont Nucrel® 0910HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating 8.7 wt% Methacrylic Acid.Nucrel® 0910HS (High-Stability) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating and extrusion lamin.. |
|||
Seal Strength | 1500 g/25 mm | 1500 g/in | seal bar 140°C. |
DuPont Nucrel® 0910HS-SR Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating
(discontinued **)< 8.7 wt% Methacrylic Acid.Nucrel® 0910HS-SR is an ethylene-methacrylic acid copolymer resin available for use in conventional and coextrusion coating equipment designed to process polyethylene resin.. |