Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 201 g/25 mm | 201 g/in | |
DuPont Teijin Films Mylar® M33 Polyester Film, 50 Gauge, PVDC Coated Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. the coating is heat sealable, and is an excellent moisture and.. |
|||
Seal Strength | 201 g/25 mm | 201 g/in | |
DuPont Teijin Films Mylar® MC2 Polyester Film, 100 Gauge (25 µm), PVDC Coated Data provided by DuPont Packaging Polymers.A polyester film with a vacuum deposited layer of aluminum on one side and overcoated on both sides with a heat sealable PVDC copolymer. The film has exce.. |
|||
Seal Strength | 201 g/25 mm | 201 g/in | |
DuPont Teijin Films Mylar® MC2 Polyester Film, 50 Gauge (14 µm), PVDC Coated Data provided by DuPont Packaging Polymers.A polyester film with a vacuum deposited layer of aluminum on one side and overcoated on both sides with a heat sealable PVDC copolymer. The film has exce.. |
|||
Seal Strength | 201 g/25 mm | 201 g/in | |
DuPont Teijin Films Mylar® M30 Polyester Film, 50 Gauge (14 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and.. |
|||
Seal Strength | 201 g/25 mm | 201 g/in | |
DuPont Teijin Films Mylar® M30 Polyester Film, 75 Gauge (21 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and.. |
|||
Seal Strength | 201 g/25 mm | 201 g/in | |
DuPont Teijin Films Mylar® M30 Polyester Film, 100 Gauge (25 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and.. |