Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.110 kN/m | 0.625 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7880 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Material 7880 is a 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for traditional.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7880HL Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 78 lb clay-coated kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abras.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7883 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Materials 7883 is a 3.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for tradition.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7883HL Computer-Imprintable Polyester Label Material Information provided by 3M |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7924 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7931 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7983 Sheet Polyester Label Material Features:Matte coating is compatible with screen printing and resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations. Variable information can be added by the end .. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | Adhesion to Polyethylene; ASTM D1000 |
3M Scotch™ 2228 Rubber Mastic Tape 3M™ Scotch™ 2228 is a conformable self-fusing rubber electrical insulating sealing tape. Scotch 2228 consist of an ethylene propylene rubber (EPR) backing coated with an aggressive, temperature-st.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7887 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |
|||
Peel Strength | 0.110 kN/m | 0.625 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7980 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |