Material Notes:
2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasion resistance in bar code applications.Quick Stick Adhesive has high tack and ultimate peel.3M Performance Label offers wide range of products for long term durability and adhesion with automotive chemical resistance and outdoor durability. Some products are UL/CSA compliant materials that can be printed by Flexographic or Screen Print processes, as well as Thermal Transfer, Digital Printing, Inkjet, Laser or Dot Matrix Printing. Available with many facestocks such as Polyester, Polypropylene and Vinyl to Pharmaceutical papers or synthetics. Please refer to individual Product Datapage for specific product details.Think 3M First for Label Materials used in these Key Markets - Automotive, Electronics, Medical Device, Outdoor Power Equipment, Health Care, Security, Government, Personal Care, Recreational Vehicle, Aerospace, Transportation, Packaging, Foam Fabrication and General Industrial.Typical 3M Performance Label Applications include Bar Code Tracking, Track and Trace, Thermal Transfer Labels, Variable Information Printing (VIP), Brand and Instruction Labels, Warning Labels, Durable Decals, Surface Protection and Masking, Over Laminate, UV Protection, Tamper Indicating, Destructable Labels, Void Message, Fraud Reduction, Laminating, Bonding and Digital Window Graphics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 20.3 microns
0.800 mil
Adhesive
58.4 microns
2.30 mil
Facestock
81.3 microns
3.20 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.09861 kN/m
0.5625 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.110 kN/m
0.625 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.18626 kN/m
1.0625 pli
Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.27391 kN/m
1.5625 pli
LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.307 kN/m
1.75 pli
HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.307 kN/m
1.75 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.31773 kN/m
1.8125 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.3287 kN/m
1.875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.3287 kN/m
1.875 pli
LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.351 kN/m
2.00 pli
LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.351 kN/m
2.00 pli
HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.3725 kN/m
2.125 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.394 kN/m
2.25 pli
LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.394 kN/m
2.25 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.4163 kN/m
2.375 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.4163 kN/m
2.375 pli
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.438 kN/m
2.50 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.438 kN/m
2.50 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.4602 kN/m
2.625 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.4602 kN/m
2.625 pli
Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.4602 kN/m
2.625 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.4602 kN/m
2.625 pli
Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.482 kN/m
2.75 pli
Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.482 kN/m
2.75 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.482 kN/m
2.75 pli
Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.49303 kN/m
2.8125 pli
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.5040 kN/m
2.875 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.5040 kN/m
2.875 pli
Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.526 kN/m
3.00 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.5478 kN/m
3.125 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.5478 kN/m
3.125 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.58068 kN/m
3.3125 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.58068 kN/m
3.3125 pli
Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.5916 kN/m
3.375 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.60259 kN/m
3.4375 pli
Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.614 kN/m
3.50 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.614 kN/m
3.50 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.64642 kN/m
3.6875 pli
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.657 kN/m
3.75 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.66833 kN/m
3.8125 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.7231 kN/m
4.125 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.73407 kN/m
4.1875 pli
Glass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.73407 kN/m
4.1875 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.745 kN/m
4.25 pli
Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.7669 kN/m
4.375 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.7669 kN/m
4.375 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.77789 kN/m
4.4375 pli
Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type #300 Acrylic
Liner 55# Densified kraft